TANG Jiajun,PEI Changchun*.Study on calculation formula for cracking moment of RAC beams based on SL 191[J].Journal of Yanbian University,2019,45(01):55-57.
基于SL191的RAC梁开裂弯矩计算公式研究
- Title:
- Study on calculation formula for cracking moment of RAC beams based on SL 191
- 文章编号:
- 1004-4353(2019)01-0055-03
- Keywords:
- cracking moment; calculation formula; RAC; cracking resistance
- 分类号:
- TU528
- 文献标志码:
- A
- 摘要:
- 研究了再生混凝土(RAC)梁开裂弯矩的计算公式.首先分析了RAC梁开裂弯矩的影响因素,然后依据20组RAC梁的试验数据和《水工混凝土结构设计规范》(SL 191—2008)给出了RAC梁开裂弯矩的计算公式,最后对该公式进行了验证.结果表明: RAC梁的开裂弯矩比普通混凝土梁低,并随着再生骨料取代率的增加而不断降低; 开裂弯矩修正系数与再生骨料取代率近似呈线性关系; 本文给出的公式计算值与试验值吻合良好.
- Abstract:
- The formula for calculating cracking moment of recycled aggregate concrete(RAC)beams was studied. Firstly, the influencing factors of cracking moment of RAC beams were analyzed. Then, based on the test data of 20 groups of RAC beams and the Design Code for Hydraulic Concrete Structures(SL 191—2008), a formula for calculating cracking moment of RAC beams was proposed. Finally, the formula was verified. The results show that the cracking moment of RAC beams is lower than that of ordinary concrete beams, and it decreases with the increase of replacement rate of recycled aggregate. The correction coefficient of cracking moment is approximately linear with replacement rate of recycled aggregate. The calculated value of the formula in this paper is in good agreement with the experimental value.
参考文献/References:
[1] 肖绪文,冯大阔,田伟.我国建筑垃圾回收利用现状及建议[J].施工技术,2015,44(10):6-8.
[2] 许成凯,裴长春.不同有机纤维组合对再生混凝土梁抗裂性影响[J].建筑科学,2017,33(1):63-67.
[3] 宋兵,李佰寿.方中空夹层钢管再生混凝土组合柱传热性能计算分析[J].延边大学学报(自然科学版),2016,42(3):252-256.
[4] 孙恒,李佰寿.玻化微珠再生混凝土柱外墙角部位的P -Temp计算分析[J].延边大学学报(自然科学版),2015,41(4):343-347.
[5] 刘洋,曾志兴,万超,等.再生陶瓷粗骨料混凝土碳化后力学性能试验研究[J].人民长江,2014,45(12):89-92.
[6] NEPOMUCENO M C S, ISIDORO R A S, CATARINO J P G. Mechanical performance evaluation of concrete made with recycled ceramic coarse aggregates from industrial brick waste[J]. Construction and Building Materials, 2018(165):284-294.
[7] 陈宗平,占东辉,徐金俊.再生粗骨料含量对再生混凝土力学性能的影响分析[J].工业建筑,2015,45(1):130-135.
[8] 曹万林,巩晓雪,叶涛萍,等.不同再生骨料取代率的再生混凝土梁受弯性能试验研究[J].自然灾害学报,2017,26(4):10-18.
[9] MAHDI Arezoumandi, ADAM Smith, JEFFERY S Volz, et al. An experimental study on flexural strength of reinforced concrete beams with 100% recycled concrete aggregate[J]. Engineering Structures, 2015(88):154-168.
[10] 张丽娟,高丹盈,王丽,等.钢纤维再生混凝土抗剪性能试验[J].土木工程与管理学报,2017,34(2):104-107.
[11] 吴瑾,丁东方,张闻.再生骨料混凝土梁抗剪性能试验研究[J].河海大学学报(自然科学版),2010,38(1):83-86.
[12] 周彬彬,孙伟民,郭樟根,等.再生混凝土梁抗剪承载力试验研究[J].四川建筑科学研究,2009,35(6):16-18.
[13] 肖建庄.再生混凝土[M].北京:中国建筑工业出版社,2008.
[14] 韦锦帆.再生混凝土梁的抗弯性能试验研究[D].北京:北京交通大学,2017.
[15] 吴瑾,丁东方,杨曦.再生混凝土梁正截面开裂弯矩分析与试验研究[J].建筑结构,2010,40(2):112-114.
[16] 宋新伟.再生混凝土梁受弯性能试验研究[D].郑州:郑州大学,2006.
[17] 陈力.再生粗骨料混凝土梁受弯性能试验研究[D].南宁:广西大学,2013.
[18] 薛丹丹.钢-聚丙烯混杂纤维再生混凝土梁抗裂性能试验研究[D].延吉:延边大学,2015.
[19] SL 191—2008 水工混凝土结构设计规范[S].北京:中国水利水电出版社,2008.
[20] 李孝忠,王庆贺,王玉银,等.再生混凝土抗折强度的影响因素及其计算方法[J].建筑结构学报,2019,40(1):155-164.
[21] 徐广舒.再生混凝土梁正截面开裂弯矩试验研究[J].混凝土,2012(6):53-56.
备注/Memo
收稿日期: 2018-11-20
*通信作者: 裴长春(1976—),男,博士,讲师,研究方向为混凝土结构理论与应用.